Scaling the Stiffness, Strength, and Toughness of Ceramic-Coated Nanotube Foams into the Structural Regime
Anna Brieland-Shoultz*, Sameh Tawfick*, Sei Jin Park* (* equal contribution), Mostafa Bedewy, Matthew R. Maschmann, Jeffery W. Baur, and A. John Hart
Advanced Functional Materials, 2014